Materia proprietatibus
Bs(T) | 1.2 |
Hc A/m) | <2 |
Tc(℃) | 570 |
Tx(℃) | 500 |
Lamination factor | >0.75 |
crassitudo (mm) | 0.020~0.035 |
λs | <2×10-6 |
opus temperatus℃ | -40~130 |
μi(High Br,0.8T) | 180,000 |
μi(Medium Br,0.4T) | 100,000 |
μi(Low Br,0.1T) | 30,000 |
damnum P(400Hz,1.0T),(W/kg) | <1.5 |
damnum P(5kHz,1.0T),(W/kg) | <15 |
damnum P(20kHz,0.5T),(W/kg) | <25 |
damnum P(100kHz,0.2T),(W/kg) | <70 |
Product speciem
1. nucleus angularis: OD-extra diametrum, ID-diameter interior & HT altitudo
2. implens coefficientem: 75
Ps: Quantumvis certae magnitudinis iuxta petitiones clientium producere potes
Product numerus | style | IN' | Turns | Diameter filum | LN | Core specification | |
10KHz mH) | 100KHz mH) | ||||||
EHC-GM02-SP151 | unum tempus | 2 | 16 | 0.55*1P | 8.0 | 1.7 | 15*10*6 |
EHC-GM05-SP152 | unum tempus | 5 | 10 | 0.9*1P | 2.9 | 0.6 | 15*10*6 |
EHC-GM05-SP201 | unum tempus | 5 | 13 | 0.9*1P | 9.0 | 1.8 | 20* 12*8 |
EHC-GM08-SP203 | unum tempus | 8 | 10 | 1.15*1P | 5.8 | 1.2 | 20* 12*8 |
EHC-GM10-SP251 | unum tempus | 10 | 16 | 1.25*1P | 7.8 | 1.6 | 25*20*10 |
EHC-GM12-SP252 | unum tempus | 12 | 11 | 1.4*1P | 7.5 | 1.6 | 25*16*10 |
EHC-GM15-SP301 | unum tempus | 15 | 13 | 1.55*1P | 9.5 | 1.9 | 30*20*10 |
EHC-GM20-SP321 | unum tempus | 20 | 11 | 1.8*1P | 7.5 | 1.6 | 32*20*10 |
EHC-GM25-SP331 | unum tempus | 25 | 9 | 1.4*2P | 6 | 1.2 | 33*23*15 |
EHC-GM30-SP401 | unum tempus | 30 | 11 | 1.8*2P | 5 | 1.1 | 40* 32*15 |
EHC-GM30-TP402 | triphase | 30 | 7 | 2.0*1P | 2.2 | 0.45 | 40* 32*15 |
EHC-GM40-SP501 | unum tempus | 40 | 9 | 2.24*2P | 4.0 | 1.0 | 50*40*20 |
EHC-GM40-TP502 | triphase | 40 | 7 | 2.24*2P | 2.5 | 0.55 | 50*40*20 |
EHC-GM60-SP502 | unum tempus | 60 | 9 | 2.8*2P | 6.0 | 1.5 | 65*50*25 |
EHC-GM60-TP502 | triphase | 60 | 6 | 2.8*2P | 2.8 | 0.65 | 65*50*25 |